Hard hard anodized aluminum, disulfided Molybdenum and Teflon (surface)
Just hard anodized coating may cause seizure if the contact surface pressure is high or fine vibration or friction occurs in places where friction occurs.
This hard anodized has a self lubrication function and succeeded in improving the wear resistance performance in Sprocket.
Molybdenum disulfide that has penetrated throughout the pores of Anodized by electrodeposition reduces the frictional resistance of the hard coating to the Large width.
There is lubrication which is used for sliding parts with no lubrication.
In friction resistance test, durability performance several times higher than standard hard anodized.
About 130% -150% improvement compared with standard Anodized.